EU/RU/BR/USA Warehosue Provides Free Shipping Service for Most Available Countries. You Can Get Speical Price Products On Each Monday of Every Month.

Your Shopping Cart Is Empty
How to deal with Supper-Clear Resin model?

How to deal with Supper-Clear Resin model?

方法/Solution

操作流程/Procedures

缺点/Shortcoming

A

推荐

Recommend

用酒精或异丙醇(IPA最佳)清洗,尽量减短清洗时间(2分钟以内)。吹干表面溶剂后进行无氧固化(20s内)(水中或者甘油中),喷砂打磨上光油。

1. Clean the model with Alcohol(IPA is better). Please control the clean time within two minutes.

2. Blow-dry the model surface with a air gun.

3. Water or glycerin cure less than 20s.

4. Polish and oil the model.

 

None

B

等待表面树脂流干,用气枪吹掉表面树脂,然后进行空气中的二次固化(30s内)。

1. Blow-dry the resin on model surface.

2. Paint evenly clear resin on the surface.

模型的细节会有点模糊

Lose some details

C

用酒精或异丙醇(IPA)清洗,尽量减短清洗时间(2分钟以内)。吹干表面溶剂,后刷一层透明树脂,空气中二次固化即可(30s)。

1. Clean the model with Alcohol(IPA is better). Please control the clean time within two minutes.

2. Blow-dry the model surface with a air gun.

3. Paint evenly clear resin on the surface.

4. Cured the surfaceless than 20s.

模型的细节会有点模糊

Lose some details

 

 

注意事项/Attention:

1. 超透树脂虽具有耐黄特性,后固化过长(诺瓦固化箱后固化时间只需要20秒),仍会导致模型轻微变黄,放入50-60℃的水中浸泡2小时左右,可减轻甚至祛除微黄。Put the model into 50-60℃ water for 2 hours can help relieving yellowing parts or even bring back to a full clear model.

 

2. 透明树脂对链式反映更加明显,请控制打印所需树脂量,打印剩余树脂建议单独存放。Clear resin is more sensitive to chain reaction. Please control your amount of usage and save the used and new resin separately. 